An secondary battery includes a cathode layer, an anode layer having an anode current collector and an anode active material layer on the anode current collector, a lithium metal layer or a lithium alloy layer between the anode current collector and the anode active material layer, wherein the lithium metal layer or the lithium alloy layer has a thickness in a range of about 10 micrometers to about 60 micrometers, and a solid electrolyte layer between the cathode layer and the anode layer, wherein the solid electrolyte is an oxide, phosphate, borate, sulfate, an oxynitride, or a combination thereof.
Claims20
A secondary battery comprising:
- a cathode layer;
- an anode layer comprising an anode current collector and a layer comprising an anode active material and a binder on the anode current collector;
- a lithium metal layer or a lithium alloy layer between the anode current collector and the anode active material layer, wherein the lithium metal layer or the lithium alloy layer has a thickness in a range of about 10 micrometers to about 60 micrometers;
- and
- a solid electrolyte layer between the cathode layer and the anode layer, wherein the solid electrolyte layer comprises;
- Li1+x+yAlxTi2−xSiyP3−yO12 wherein 0<x<2, and 0≤y<3, Pb(Zr1−aTia)O3 wherein 0≤a≤1, Pb1−xLaxZr1−yTiyO3 wherein 0≤x<1, and 0≤y<1, Pb(Mg1/3Nb2/3)O3—PbTiO3, Li3PO4, LixTiy(PO4)3 wherein 0<x<2, and 0<y<3, LixAlyTiz(PO4)3 wherein 0<x<2, 0<y<1, and 0<z<3, Li1+x+y(AlaGa1−a)x(TibGe1−b)2−xSiyP3−yO12 wherein 0≤x≤1, 0≤y≤1, 0≤a≤1, and 0≤b≤1, LixLayTiO3 wherein 0<x<2, and 0<y<3, LiAlO2, a Li2O—Al2O3—SiO2—P2O5—TiO2—GeO2, Li3+xLa3M2O12 wherein M is Te, Nb, Zr, or a combination thereof, and 0≤x≤10, Li7La3Zr2−xTaxO12 wherein 0<x<2, or a combination thereof.
A method of preparing a secondary battery, the method comprising:
- providing a solid electrolyte layer on a substrate;
- acid-treating the solid electrolyte layer to provide an acid-treated solid electrolyte layer;
- and
- stacking the acid-treated solid electrolyte layer between a cathode layer and an anode layer, such that a binding strength between the solid electrolyte layer and the anode layer is in a range of about 14 millinewtons per millimeter to about 100 millinewtons per millimeter.