US 2025/0210280 A1Published application
Physically activated carbon for all-solid-state supercapacitors and methods of preparation thereof
AssigneeKing Fahd University of Petroleum and Minerals
InventorsAziz AHMAD, Mohammed Ashraf G. GONDAL, Atif ALZAHRANI
Life of this patent
Estimating the term…
Abstract
An electrode including a substrate, a binding compound, date seed mesoporous carbon, and a conductive carbon (CC) other than the date seed mesoporous carbon. The date seed mesoporous carbon has a surface area of 600-800 m2/g, an average pore size of 1-5 nm, and a sheet morphology. A mixture of the binding compound, the date seed mesoporous carbon, and the conductive carbon other than the date seed mesoporous carbon is coated on the surface of the substrate.
Claims20
1:
- An electrode comprising:
- a substrate;
- a binding compound,
- date seed mesoporous carbon;
- and
- a conductive carbon other than the date seed mesoporous carbon,
- wherein the date seed mesoporous carbon has a surface area of 600-800 m2/g, and an average pore size of 1-5 nm,
- wherein the date seed mesoporous carbon has a sheet morphology, and
- wherein a mixture of the binding compound, the date seed mesoporous carbon, and the conductive carbon other than the date seed mesoporous carbon is coated on a surface of the substrate.
6 more elements
2:
- The electrode of claim 1, wherein the mixture comprises 1-10 wt. % of the binding compound, 60-80 wt. % of the date seed mesoporous carbon, and 10-30 wt. % conductive carbon other than the date seed mesoporous carbon, based on a total weight of the mixture.
3:
- The electrode of claim 1, wherein the date seed mesoporous carbon comprises amorphous graphitic carbon.
4:
- The electrode of claim 1, wherein sheets of the date seed mesoporous carbon have an average width of 50-200 nm.
5:
- The electrode of claim 1, wherein sheets of the date seed mesoporous carbon have an average length of greater than 200 nm.
6:
- The electrode of claim 1, wherein sheets of the date seed mesoporous carbon stack on top of one another.
7:
- The electrode of claim 1, wherein the date seed mesoporous carbon comprises C, N and O.
8:
- The electrode of claim 1, wherein pores of the date seed mesoporous carbon are present on a surface of the sheets.
9:
- The electrode of claim 1, wherein the date seed mesoporous carbon comprises both mesopores and micropores.
10:
- The electrode of claim 1, wherein the binding compound is a fluorinated polymer.
11:
- The electrode of claim 1, wherein the conductive carbon other than the date seed mesoporous carbon is at least one selected from the group consisting of graphite, activated carbon, reduced graphene oxide, carbon nanotubes, carbon nanofibers, and carbon black.
12:
- The electrode of claim 1, wherein the substrate is made from at least one material selected from the group consisting of stainless steel, aluminum, nickel, copper, platinum, zinc, tungsten, and titanium.
13:
- The electrode of claim 1, having a specific capacitance of 100-150 F/g at a scan rate of 5 mV/s.
14:
- The electrode of claim 1, wherein the date seed mesoporous carbon is made by a method comprising:
- pulverizing date seeds into a date seed powder;
- pyrolyzing the date seed powder at a temperature of 500-700° C. under an inert atmosphere to form a pyrolyzed date seed powder;
- pulverizing the pyrolyzed date seed powder into a refined date seed powder;
- and
- activating the refined date seed powder at a temperature of 700-1,000° C. under carbon dioxide to form the date seed mesoporous carbon.
3 more elements
15:
- The electrode of claim 14, wherein the method does not include a chemical activation agent.
16:
- A supercapacitor, comprising:
- two of the electrodes of claim 1;
- and
- a solid-state electrolyte,
- wherein the electrodes are disposed facing each other, and
- wherein the solid-state electrolyte is present between the electrodes to form the supercapacitor.
3 more elements
17:
- The supercapacitor of claim 16, wherein the solid-state electrolyte comprises a polymer and a base.
18:
- The supercapacitor of claim 16, wherein the solid-state electrolyte comprises polyvinyl alcohol and KOH.
19:
- The supercapacitor of claim 16, having a power density of 70-100 W/kg.
20:
- The electrode of claim 1, wherein the date seed mesoporous carbon is obtained by first devolatizing a date seed biomass at a temperature of at least 600° C. under an inert atmosphere to form a devolatized date seed powder;
- then
- activating the devolatized date seed powder at a temperature of at least 850° C. in an carbon dioxide atmosphere to form the date seed mesoporous carbon.