Back to results
US 2025/0207265 A1Published application
Composition for protecting copper surface, and method for producing semiconductor intermediate and semiconductor using same
AssigneeMitsubishi Gas Chemical Company, Inc.
InventorToshiyuki OIE
Life of this patent
Estimating the term…
Abstract
Provided are a composition for protecting a copper surface, a method for producing a semiconductor intermediate using the composition, and a method for producing a semiconductor using the composition. The composition contains a solvent and at least one copper surface protectant chosen from compounds represented by formulae (1) to (3) below and salts thereof:
Claims12
1:
- A composition for protecting a copper surface, the composition comprising:
- at least one copper surface protectant selected from the group consisting of compounds represented by formulae (1) to (3) and salts thereof:
- in formulae (1) to (3), R is a substituted or unsubstituted alkyl group having 3 to 30 carbon atoms or a substituted or unsubstituted aryl group having 6 to 30 carbon atoms;
- and
- a solvent.
2 more elements
2:
- The composition according to claim 1, wherein the copper surface protectant contains a compound represented by formula (1) and/or a salt thereof.
3:
- The composition according to claim 1, wherein R is a substituted or unsubstituted alkyl group having 3 to 30 carbon atoms.
4:
- The composition according to claim 1, further comprising a pH adjusting agent.
5:
- The composition according to claim 4, wherein the pH adjusting agent contains at least one selected from the group consisting of sodium hydroxide and potassium hydroxide.
6:
- The composition according to claim 1, which has a pH of 2.5 to 5.5.
7:
- The composition according to claim 1, which is used for producing a semiconductor.
8:
- A method for producing a first semiconductor intermediate, the method comprising:
- step (1):
- bringing the composition according to claim 1 into contact with a copper-containing layer in a first semiconductor having the copper-containing layer to form a copper surface protective layer.
9:
- The method according to claim 8, further comprising:
- washing the copper-containing layer of the first semiconductor with a washing liquid before the step (1).
10:
- The method according to claim 9, wherein the washing liquid contains at least one selected from the group consisting of hydrofluoric acid, sulfuric acid, nitric acid, and ammonia.
11:
- A method for producing a semiconductor, the method comprising:
- removing a copper surface protective layer of a first semiconductor intermediate produced by the method according to claim 8 to expose a copper-containing layer;
- and
- bonding the exposed copper-containing layer to a metal-containing layer in a second semiconductor intermediate including the metal-containing layer to form a copper-containing bonding layer.
1 more element
12:
- The composition according to claim 5, which has a pH of 2.5 to 5.5.