US 2025/0179223 A1Published application
Method for reduction of discoloration in latex polymers
AssigneeSabic Global Technologies B.V.
InventorsNasser Mansour Alsubaie, Dejin Li
Life of this patent
Estimating the term…
Abstract
A method comprising providing a polymer latex comprising particles of polymer in aqueous dispersion, adding a peroxide in an amount of 0.005 to 5, preferably 0.01 to 4, parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 8.5, preferably at least 9, and, after the contacting, coagulating the polymer latex.
Claims20
A method comprising
- providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise polymers of one or more of vinyl aromatic monomers, acrylic monomers,
- adding a peroxide in an amount of 0.005 to 5 parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 8.5, and,
- after adding the peroxide, coagulating the polymer latex,
- wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 2 minutes.
1 more element
A method comprising
- providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise a copolymer of a styrenic monomer, an acrylonitrile monomer, and a conjugated diene monomer,
- adding a peroxide comprising hydrogen peroxide in an amount of 0.005 to 5 parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 9 and at most 12, and,
- after adding the peroxide, coagulating the polymer latex,
- wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 10 minutes and up to 1 hour.
1 more element
A method comprising
- providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise an acrylonitrile-butadiene-styrene copolymer;
- adding a peroxide comprising hydrogen peroxide in an amount of 0.01 to 0.5 part by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 9 and at most 12, and
- after adding the peroxide, coagulating the polymer latex,
- wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 10 minutes and up to 1 hour,
- wherein the polymer latex comprises 30 to 45 weight percent solids in an aqueous solution.
2 more elements