Low-k feature formation processes and structures formed thereby
AssigneeTaiwan Semiconductor Manufacturing Company, Ltd.
InventorsWan-Yi Kao, Chung-Chi Ko
Life of this patent
Estimating the term…
Abstract
Embodiments of the present disclosure relate to a method of forming a low-k dielectric material, for example, a low-k gate spacer layer in a FinFET device. The low-k dielectric material may be formed using a precursor having a general chemical structure comprising at least one carbon atom bonded between two silicon atoms. A target k-value of the dielectric material may be achieved by controlling carbon concentration in the dielectric material.
Claims20
A method of manufacturing a semiconductor device, the method comprising:
- forming a gate structure over a semiconductor fin;
- forming at least one dielectric material having a density of between 1 g/cm3 and 3 g/cm3, a non-zero carbon concentration less than 30 at. % and a non-zero nitrogen concentration of less than 3 at. %;
- and
- forming a gate contact adjacent to the gate structure after the forming the at least one dielectric material, the at least one dielectric material being located between the gate contact and the gate structure.
A method of manufacturing a semiconductor device, the method comprising:
- forming a gate located between a pair of source/drain regions over a semiconductor substrate;
- forming a dielectric layer over the source/drain regions;
- and
- forming a contact extending through the dielectric layer to be in physical contact with a first one of the pair of source/drain regions, wherein a spacer is located adjacent to the contact, the spacer having a density of between 1 g/cm3 and 3 g/cm3, a non-zero carbon concentration less than 30 at. % and a non-zero nitrogen concentration of less than 3 at. %.
A method of manufacturing a semiconductor device, the method comprising:
- forming a first source/drain region extending out of a semiconductor substrate;
- forming a first dielectric material in physical contact with each of the semiconductor substrate, the first source/drain region, a gate dielectric, and a gate electrode;
- forming a second dielectric material in physical contact with each of the source/drain region, the first dielectric material, and a contact etch stop layer, wherein after the forming the second dielectric material the contact etch stop layer is in physical contact with an overlying first dielectric layer, the second dielectric material having a density of between 1 g/cm3 and 3 g/cm3, a non-zero carbon concentration less than 30 at. % and a non-zero nitrogen concentration of less than 3 at. %;
- and
- forming a contact extending through the first dielectric layer and the contact etch stop layer to make physical contact with a silicide region of the first source/drain region.
Dependencies are inferred from the claim text.