Lithium-ion secondary battery
AssigneeToyota Jidosha Kabushiki Kaisha
InventorsRyo ASAKURA, Shinya SHIOTANI, Sakina KANEKO
Life of this patent
Estimating the term…
Abstract
A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions includes a cathode layer, an anode layer and an electrolyte layer between the cathode layer and the anode layer, the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions, the anode layer includes a silver (Ag) element, a tin (Sn) element, and a lithium (Li) element, and a molar ratio of the Sn element to the Ag element (Sn/Ag) contained in the anode layer is 0.09 or higher and 0.17 or lower.
Claims5
A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions, the lithium-ion secondary battery comprising:
- a cathode layer;
- an anode layer;
- and
- an electrolyte layer between the cathode layer and the anode layer, wherein:
- the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions;
- the anode layer includes a silver element, a tin element, and a lithium element;
- and
- a molar ratio of the tin element to the silver element contained in the anode layer is 0.09 or higher and 0.17 or lower.
A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions, the lithium-ion secondary battery comprising:
- a cathode layer;
- an anode layer;
- and
- an electrolyte layer between the cathode layer and the anode layer, wherein:
- the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions;
- the anode layer includes a metal tin layer containing elemental tin, and a metal silver layer containing elemental silver in order from a side of the electrolyte layer;
- and
- a molar ratio of a tin element to a silver element contained in the anode layer is 0.09 or higher and 0.17 or lower.
Dependencies are inferred from the claim text.