Abstract
The present invention relates generally to resistant dextrins and methods of making resistant dextrins. In particular, the present invention relates to resistant dextrins having physical properties desirable in, at least, products for the food and beverage industry. In particular, the present invention relates to methods of making the resistant dextrins having physical properties desirable in, at least, products for the food and beverage industry.
Claims20
A resistant dextrin in particulate form, having:
- a SPAN of at most 2.7;
- and
- a specific surface area of from 0.05 to 0.20 m2/g, as measured by the Brunauer-Emmett-Teller (BET) adsorption method.
(canceled)
(canceled)
A method of forming a resistant dextrin in liquid form, the method comprising:
- (a) providing a saccharide feed comprising at least 35 weight % on a dry solid basis of dextrose and/or dextrose oligomers;
- (b) heating the saccharide feed to a temperature of at least 60° C.;
- (c) adding an acidifying catalyst to form an acidic composition;
- (d) heating the acidic composition up to at least 120° C.;
- (e) injecting the acidic composition through a first microdevice to react the dextrose and/or dextrose oligomers with the acid catalyst in the presence of water for a time sufficient to produce a first reacted composition wherein at least 60 weight % of the dextrose and/or dextrose oligomers have reacted, and wherein the first reacted composition comprises from 60 to 90 weight % weight dry solids;
- (f) extracting the water from the first reacted composition to obtain a water-depleted composition comprising at least 90 weight % dry solids;
- (g) injecting the water-depleted composition through a second microdevice to react any non-reacted dextrose and/or dextrose oligomers with the acid catalyst at a temperature of at least 160° C. for a time sufficient to produce a second reacted composition wherein at least 90 weight % of the dextrose and/or dextrose oligomer have reacted, and wherein the second reacted composition comprises from 60 to 80 weight % dry solids;
- and
- (h) refining the second reacted composition to form the resistant dextrin in liquid form.