Lithium-containing precursor material, with a chemical formula of LixMyD, wherein M is at least one of Ni, Co, Mn, Al, or Mg, and D is one or more of CO32−, OH−, or C2O42−;
- 0.2<x<0.9, 0.25<y<0.9, and 0.5<x/y<1.5;
- a 2θ diffraction angle of the lithium-containing precursor material has following characteristic peaks in an XRD pattern of a Cu target Kα1, the characteristic peaks P1 at 20°-22°, and the characteristic peak P2 at 31°-33°, and peak intensities of the characteristic peak p1 and the characteristic peak p2 meet the following relational expression:
- 0<(p1/p2)≤10.