METHOD FOR PRODUCING CALCINED PRODUCT COMPRISING gamma-2CaOSiO2
AssigneeTokuyama Corporation
InventorMasami OTA
Life of this patent
Estimating the term…
Abstract
By preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2 O3 after heating at 1000° C. of 5.0 mass % or less, and calcining at a calcination temperature of 1350° C. to 1600° C., it is possible to efficiently use waste materials as a part of raw materials, and to obtain a calcined product that comprises almost an equivalent amount of γ-2CaO·SiO2 as conventional can be obtained.
Claims4
A method of producing a calcined product comprising γ-2CaO·SiO2, the method comprising preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2 O3 after heating at 1000° C. of 5.0 mass % or less, and calcining at a calcination temperature of 1350° C. to 1600° C.
Dependencies are inferred from the claim text.