Nickel oxide sol-gel ink
AssigneeCubicPV Inc.
InventorsMichael D. Irwin, Erin Sanehira
Life of this patent
Estimating the term…
Abstract
A method for preparing a nickel oxide precursor ink comprising: preparing a solvent comprising diols and alcohol amines; adding nickel nitrate into the solvent to form a nickel nitrate containing solution; adding at least one metal acetate into the nickel nitrate containing solution to form a nickel nitrate and metal acetate containing solution; adding water to the nickel nitrate and metal acetate containing solution to form a nickel oxide precursor mixture; heating the nickel oxide precursor mixture to 60 to 75 Celsius; and cooling the nickel oxide precursor mixture to form the nickel oxide precursor ink.
Claims1
A method for depositing a nickel oxide layer comprising:
- preparing a substrate;
- depositing a nickel oxide precursor ink onto the substrate, wherein the nickel oxide precursor ink comprises:
- a solvent comprising diols, alcohol amines, and water;
- Ni(NO3)2·6H2O;
- and
- at least one metal acetate selected from the group consisting of Ni(CH3CO2)2·4H2O and Cu(CH3CO2)2·1H2O;
- annealing the nickel oxide precursor ink at a temperature between 250° to 400° Celsius for between 10 minutes and 6 hours;
- and
- cooling the nickel oxide precursor ink to form the nickel oxide layer.
Dependencies are inferred from the claim text.