A carbon matrix, wherein the carbon matrix has a cross-linked porous structure internally, and a value of flexibility C2 of the carbon matrix satisfies 0.8≤C2≤2 or 1.2≤C2≤1.8, the flexibility being measured by applying a pressure of 2t to the carbon matrix, holding the pressure for 10s and releasing the pressure for 100s, repeating until the pressure is held and released for 20 times, recording a compacted density P5 at the 1st pressure holding, a compacted density P6 at the 20th pressure holding, a compacted density P7 at the 1st pressure releasing, and a compacted density P8 at the 20th pressure releasing, and calculating C2=(P8−P7)/(P6−P5),
- wherein M2 is defined as P6−P5, and N2 is defined as P8−P7, wherein 0.04≤M2≤0.18 and 0.04≤N2≤0.08;
- or wherein the carbon matrix comprises a first region and a second region in sequence along a direction extending from a center to a surface, wherein a volume of the second region is twice a volume of the first region, and a ratio of a number of pores with a pore size of 2 nm to 1000 nm in the first region to a number of pores with a pore size of 2 nm to 1000 nm in the second region is greater than 1;
- or wherein a ratio of a number of pores with a pore size of 2 nm to 500 nm in the first region to a number of pores with a pore size of 2 nm to 500 nm in the second region is greater than 1;
- or wherein a ratio of a number of pores with a pore size of 2 nm to 200 nm in the first region to a number of pores with a pore size of 2 nm to 200 nm in the second region is greater than 1.