Cellulosic fiber material and process
AssigneePaperShell AB
InventorsAnders BREITHOLTZ, Mathieu GUSTAFSSON APLEHAG
Life of this patent
Estimating the term…
Abstract
The present invention relates to a cellulosic fiber substrate, comprising at least one top surface and at least one bottom surface. The cellulosic fiber substrate further comprises 60 to 90 wt % of cellulosic fibers having a length of maximum 10 mm, 0 to 10% of an acidic curing catalyst and 10 to 40 wt % of a binding agent selected form the group consisting of: cellulose, hemicellulose, furan, lignin and combinations thereof.
Claims22
A cellulosic fiber substrate, comprising:
- at least one top surface,
- at least one bottom surface,
- wherein, the cellulosic fiber substrate further comprises:
- 60 to 90 wt % of cellulosic fibers having a length of maximum 10 mm, 0 to 10% of an acidic curing catalyst and
- 10 to 40 wt % of a binding agent selected form the group consisting of:
- cellulose, hemicellulose, furan, lignin and combinations thereof.
Load bearing 3D article according to claim 10, wherein the load bearing article has a tensile strength least of at least 40 MPa, preferably at least 50 MPa, more preferably at least 100 MPa.
A method for manufacturing a cellulosic fiber substrate comprising at least one top surface and one bottom surface, the method comprising the steps of:
- a) providing at least one sheet of cellulosic fibers having a maximum length of 10 mm;
- b) impregnating the at least one sheet of cellulosic fibers with a mix of an acidic curing catalyst and a binding agent selected form the group consisting of:
- cellulose, hemicellulose, furan, lignin and combinations thereof, to obtain at least one sheet of impregnated cellulosic fibers;
- c) pre-curing the at least one sheet of impregnated cellulosic fibers by applying heat in the range of 50-300° C., thus obtaining a prepreg;
- d) arranging one or more prepregs in a stack;
- e) pressing said stack in a pressing tool at a pressure of at least 7 kg/cm2, preferably at least 25 kg/cm2, more preferably at least 30 kg/cm2 and the temperature of at least 60° C., preferably at least 140° C., more preferably at least 150° C. during a time period of at least 10 seconds, preferably at least one minute, more preferably at least two minutes, thus obtaining a cellulosic fiber substrate having at least one top surface and one bottom surface.
Dependencies are inferred from the claim text.