Surface-treated silica particle dispersion sol and production method therefor
AssigneeMitsubishi Materials Electronic Chemicals Co., Ltd.
InventorYuta Yamamoto
Life of this patent
Estimating the term…
Loading patent…
AssigneeMitsubishi Materials Electronic Chemicals Co., Ltd.
InventorYuta Yamamoto
Estimating the term…
This surface-treated silica particle dispersion sol is formed by dispersing a group of colloidal silica particles in a hydrophobic solvent, the colloidal silica particles being composed of an average number of 4 to 300 spherical primary particles, chainly connected to have an average length of 35 nm to 1,800 nm, and the particle surfaces being coated with a silane coupling agent or the like having a functional group such as a vinyl group. The average particle diameter of the spherical primary particles is 6 nm to 20 nm and the average aspect ratio of the spherical primary particles is in the range of 1.0 to 1.3. The content ratio of impurities of K, Na, or NH3 per colloidal silica particle is 3,500 ppm by mass or less and the content ratio of impurities of alkaline earth metals or aluminum is less than 1 ppm by mass.
A surface-treated silica particle dispersion sol formed by dispersing a group of colloidal silica particles in a hydrophobic solvent, the colloidal silica particles being composed of an average number of 4 to 300 spherical primary particles, as observed with a field emission-type scanning electron microscope, chainly connected to have an average length of 35 nm to 1,800 nm, and the surfaces of the particles being coated with a silane coupling agent having a functional group which is a vinyl group, a methyl group, an epoxy group, a styryl group, or a methacrylic group, or coated with a titanate-based coupling agent or an aluminate-based coupling agent,
Dependencies are inferred from the claim text.