Indigo and ring dyeing process using sulfur dye as barrier, and material produced thereby
AssigneeCleanKore, LLC
InventorsDarryl J. COSTIN, JR., Alpesh PATEL
Life of this patent
Estimating the term…
Abstract
A method of ring dyeing a yarn includes the steps of providing a cellulosic yarn chosen from the group consisting of open-end yarns and ring yarns. The yarn is immersed in only one sulfur dye box, the sulfur dye box having a sulfur concentration of 1 to 50 grams/liter. The yarn is skyed for less than 30 seconds after removal from the sulfur dye box. The yarn is rinsed in water after skying. The yarn is dyed in an indigo dye bath, with the indigo dye bath maintained at a pH of 10.8 and 12.8. The yarn is skyed after removal from the indigo dye box.
Claims24
A method of ring dyeing a yarn, comprising the steps of:
- providing a cellulosic yarn chosen from the group consisting of open-end yarns and ring yarns;
- immersing the yarn in only one sulfur dye box, the sulfur dye box having a sulfur concentration of 1 to 50 grams/liter;
- skying the yarn for less than 30 seconds after removal from the sulfur dye box;
- rinsing the yarn water after skying;
- dyeing the yarn in an indigo dye bath, the indigo dye bath maintained at a pH between 10.8 and 12.8;
- and
- skying the yarn after removal from the indigo dye box.
A method of ring dyeing a yarn, comprising the steps of:
- providing a cellulosic yarn chosen from the group consisting of open-end yarns and ring yarns;
- immersing the yarn in only one sulfur dye bath for between 6 to 14 seconds, the sulfur dye bath having a sulfur concentration of 1 to 50 grams/liter;
- skying the yarn for less than 30 seconds after removal from the sulfur dye bath;
- rinsing the yarn in water after skying;
- thereafter dyeing the yarn in an indigo dye solution for between 6 to 14 seconds, the dye solution maintained at a pH of 10.8 to 12.8;
- and
- thereafter skying the yarn for 30 to 140 seconds.
A method of dyeing yarn, comprising the steps of:
- Providing a cellulosic yarn;
- Immersing the yarn in a caustic solution;
- Rinsing the yarn in water to remove excess caustic;
- Immersing the yarn is sulfur dyes for a limited immersion time;
- Skying the yarn after dyeing for a limited time to minimize air oxidation of the dye;
- Rinsing the yarn in water to oxidize the sulfur dyes and remove unreacted dyes from the yarn;
- Immersing the yarn in indigo for a limited immersion time;
- and
- Skying the yarn for a period sufficient to oxidize the indigo dye.
Dependencies are inferred from the claim text.