Back to results
US 2024/0343626 A1Published application
Glass material producing method and glass material
AssigneeNippon Electric Glass Co., Ltd.
InventorTomoko ENOMOTO
Life of this patent
Estimating the term…
Abstract
Provided is a method for producing a glass material whereby a glass material less likely to undergo solarization can be obtained. A method for producing a glass material includes the steps of: preparing a glass; and subjecting the glass to heat treatment for six or more hours at a temperature of not lower than (Tg−70°) C and not higher than (Tg+40°) C where a glass transition point of the glass is represented as Tg (° C.).
Claims8
1:
- A method for producing a glass material, the method comprising the steps of:
- preparing a glass;
- and
- subjecting the glass to heat treatment for six or more hours at a temperature of not lower than (Tg−70°) C and not higher than (Tg+40°) C where a glass transition point of the glass is represented as Tg (° C.).
1 more element
2:
- The method for producing a glass material according to claim 1, wherein the glass contains, in terms of % by mole, not less than 50% La2O3+Gd2O3+Y2O3+Yb2O3+Ga2O3+TiO2+ZrO2+Nb2O5+Ta2O5+WO3 and not more than 50% B2O3+SiO2+P2O5+GeO2.
3:
- The method for producing a glass material according to claim 1, wherein the glass contains, in terms of % by mole, 10% or more La2O3.
4:
- The method for producing a glass material according to claim 1, wherein the step of preparing a glass comprises the steps of:
- heating a block of glass raw material held levitated, thus obtaining a molten glass melted from the block of glass raw material by the heating;
- and
- cooling the molten glass to obtain a glass.
1 more element
5:
- The method for producing a glass material according to claim 1, the method being a method for producing a glass material for use as an optical glass material.
6:
- A glass material containing, in terms of % by mole, not less than 50% La2O3+Gd2O3+Y2O3+Yb2O3+Ga2O3+TiO2+ZrO2+Nb2O5+Ta2O5+WO3 and not more than 50% B2O3+SiO2+P2O5+GeO2,
- wherein, when the glass material is subjected to light irradiation of light having a wavelength of 280 nm to 400 nm at an irradiance of 0.1 mW/cm2 to 10 mW/cm2 for 24 hours to 100 hours, an absolute value Δb* of a difference between a first chromaticity b* of the glass material before the light irradiation in an L*a*b* color system and a second chromaticity b* of the glass material after the light irradiation in the L*a*b* color system is 0.5 or less.
7:
- The glass material according to claim 6 containing, in terms of % by mole, 10% or more La2O3.
8:
- The glass material according to claim 6 being an optical glass material.