A composition comprising (a1) a polyether polyol, (a2) a polyolefine polyol and (a3) a polyester polyol obtainable by epoxidation of an unsaturated fatty acid ester and subsequent ring-opening reaction with a compound containing active hydrogen, can be used for the preparation of PUR foam which distinguishes by low-temperature flexibility and low dielectric loss and is suitable for filling the gap between the condenser core and the outer composite or porcelain insulator in the manufacture of resin impregnated paper (RIP) bushings.
Claims13
A process for producing a polyurethane foam by reacting a polyol component with a polyisocyanate, in the presence of a blowing agent, wherein the polyol component comprises based on the weight of the composition,
- (a) a polyether polyol,
- (b) 30-70% by weight of a polyolefin polyol, and
- (c) a polyester polyol obtained by epoxidation of an unsaturated fatty acid ester and subsequent ring-opening reaction with a compound containing active hydrogen.
A process for producing a polyurethane foam by reacting a polyol component with a polyisocyanate, in the presence of a blowing agent, wherein the polyol component comprises,
- (a) a polyether polyol,
- (b) a polyolefin polyol,
- (c) a polyester polyol obtained by epoxidation of an unsaturated fatty acid ester and subsequent ring-opening reaction with a compound containing active hydrogen, and
- (d) a polysiloxane-polyoxyalkylene block copolymer
- wherein the polyolefin polyol comprises at least one of the compounds represented by formulas (1) and (2), and
- wherein x, y, z, v and w represent the percentages of the structural units and denote the following ranges:
- x=10 to 70%, y=15 to 70%, z=10 to 30%, v=10-75%, w=25-90%, with the proviso x+y+z=100% and v+w=100%.
A process for producing a polyurethane foam by reacting a polyol component with a polyisocyanate, in the presence of a blowing agent, wherein the polyol component comprises,
- (a1) 5-30% by weight of a polyether polyol,
- (a2) 35-65% by weight of a polyolefin polyol,
- (a3) 10-50% by weight of a polyester polyol obtained by epoxidation of an unsaturated fatty acid ester and subsequent ring-opening reaction with a compound containing active hydrogen, and
- (a4) a polysiloxane-polyoxyalkylene block copolymer
- wherein the polyolefin polyol comprises at least one of the compounds represented by formulas (1) and (2):
- wherein x, y, z, v and w represent the percentages of the structural units and denote the following ranges:
- x=10 to 70%, y=15 to 70%, z=10 to 30%, v=10-75%, w=25-90%, with the proviso x+y+z=100% and v+w=100% and
- (B) a polyisocyanate comprising polymeric methylene-diphenyldiisocyanate.
An encapsulation material for electrical components wherein the encapsulation material comprises,
- (a) a polyether polyol,
- (b) a polyolefin polyol, and
- (c) a polyester polyol obtainable obtained by epoxidation of an unsaturated fatty acid ester and subsequent ring-opening reaction with a compound containing active hydrogen, and
- (d) a polyisocyanate.