Hexagonal boron nitride powder and method for producing same, and cosmetic preparation and method for producing same
AssigneeDenka Company Limited
InventorRyuki MATSUI
Life of this patent
Estimating the term…
Loading patent…
AssigneeDenka Company Limited
InventorRyuki MATSUI
Estimating the term…
A hexagonal boron nitride powder, in which an attenuation rate of a positive charge is higher than an attenuation rate of a negative charge when the attenuation rates of the positive and negative charges determined through charge attenuation measurement are compared with each other. A method for producing a hexagonal boron nitride powder includes: a calcination step of firing a raw material powder containing a boron-containing compound powder and a nitrogen-containing compound powder at 600° C. to 1300° C. in an atmosphere of an inert gas, ammonia gas, or a mixed gas thereof to obtain a calcined product containing hexagonal boron nitride; and a firing step of heating and firing a mixed powder containing the calcined product and an aid at 1900° C. to 2100° C. for 10 to 50 hours in an atmosphere of an inert gas, ammonia gas, or a mixed gas thereof.
A hexagonal boron nitride powder,
A method for producing a hexagonal boron nitride powder, the method comprising:
Dependencies are inferred from the claim text.