Sulfide-based solid electrolyte powder and method for producing same
AssigneeAGC Inc.
InventorsNaoki FUJII, Osamu HOMMA, Naoki MAEDA
Life of this patent
Estimating the term…
Abstract
The present invention relates to a sulfide solid electrolyte powder to be used for a lithium-ion secondary battery, and the sulfide solid electrolyte powder includes: at least one of a crystal phase including Li, P, and S, and an amorphous phase including Li, P, and S, in which a 1H-NMR intensity is 0.3 or more, and a BET specific surface area (m2/g) and the 1H-NMR intensity satisfy a relationship of 2≤(BET specific surface area×1H-NMR intensity).
Claims9
A sulfide solid electrolyte powder to be used for a lithium-ion secondary battery, the sulfide solid electrolyte powder comprising:
- at least one of a crystal phase comprising Li, P, and S, and an amorphous phase comprising Li, P, and S, wherein
- a 1H-NMR intensity is 0.3 or more,
- a BET specific surface area (m2/g) and the 1H-NMR intensity satisfy a relationship of 2≤(BET specific surface area×1H-NMR intensity), and
- the 1H-NMR intensity is normalized under the following conditions:
- measurement is made using adamantane as an external standard, and a chemical shift position having a highest intensity in an obtained 1H-NMR spectrum is normalized to 1.91 ppm;
- a sample is prepared by adding and mixing 2 mass % of adamantane as an internal standard to the sulfide solid electrolyte powder;
- and in a 1H-NMR spectrum of the sample obtained under conditions of a probe:
- a probe for 2.5 mm solid, a measurement condition:
- a single pulse method, a pulse width:
- 2.0 μs, an observation center:
- 8.0 ppm, an observation width:
- 40 ppm, a relaxation delay:
- 5 sec, a cumulative number:
- 64, and a rotation speed:
- 20 kHz, when an intensity of a peak derived from adamantane that is the internal standard and observed at 1.91 ppm is set to 1.7, an intensity of a peak observed in a range of 1.0±0.2 ppm is normalized assuming that the 1H-NMR intensity is 1.0.
A method for producing a sulfide solid electrolyte powder to be used for a lithium-ion secondary battery, the method comprising, in order:
- obtaining a sulfide solid electrolyte comprising at least one of a crystal phase comprising Li, P, and S, and an amorphous phase comprising Li, P, and S;
- pulverizing the sulfide solid electrolyte to obtain a powder;
- and
- heating and drying the powder, wherein
- the pulverizing is performed using a non-aqueous organic solvent,
- a concentration of moisture contained in the non-aqueous organic solvent is more than 5 ppm and 200 ppm or less, and
- a moisture concentration in a heating space in the heating and drying is more than 5 ppm and 300 ppm or less.
Dependencies are inferred from the claim text.