Carrier core material and electrophotographic development carrier using same and electrophotographic developer
AssigneesDowa Electronics Materials Co., Ltd., Dowa IP Creation Co., Ltd.
InventorShinya SASAKI
Life of this patent
Estimating the term…
Loading patent…
AssigneesDowa Electronics Materials Co., Ltd., Dowa IP Creation Co., Ltd.
InventorShinya SASAKI
Estimating the term…
A carrier core material includes ferrite particles, contains CaSiO3, and has a true density at least equal to 3.5 g/cm3 and at most equal to 4.5 g/cm3. A particle strength index calculated from formula (1) is preferably at most equal to 1.5% by volume. (1): Particle strength index=V2−V1 (In the formula, V1: cumulative value (% by volume) of particle size 22 μm or less in cumulative particle size distribution of carrier core material before crushing test, and V2: cumulative value (% by volume) of particle size 22 μm or less in cumulative particle size distribution of carrier core material after crushing test) Crushing test conditions: 30 g of carrier core material crushed using a sample mill for 60 seconds at a rotational speed of 14000 rpm.
A carrier core material formed of ferrite particles, the carrier core material comprising: