Process for overspray-free application of a resin composition and resin compositions for use in the process
AssigneeAllnex Netherlands B.V.
InventorsElwin Aloysius Cornelius Adrianus DE WOLF, Martin BOSMA
Life of this patent
Estimating the term…
Abstract
The invention relates to a process for overspray-free application of a non-aqueous thixotropic resin composition on a substrate surface and to non-aqueous thixotropic resin compositions for use in the process comprising a resin and a thixotropy agent comprising polyurea particles characterised in that the resin composition has a high-shear viscosity HSV measured at a shear rate of 1000±50 s−1 that is lower than 100 mPa·s and a creep compliance Jmax measured after 300 seconds using a creep stress of 1.0 Pa of lower than 250 Pa−1.
Claims20
A process for overspray-free application of a resin composition on a substrate surface comprising
- a. Providing a resin composition,
- b. Providing an overspray-free applicator comprising a print head comprising a plate comprising a plurality of perforated holes,
- c. Ejecting a plurality of droplet streams or jet streams of the resin composition from the plurality of holes on the substrate surface forming a layer of the resin composition,
- wherein the resin composition is a non-aqueous thixotropic resin composition comprising a resin and a thixotropy agent comprising polyurea particles characterised in that the resin composition has
- a high-shear viscosity HSV measured at 23° C. at a shear rate of 1000±50 s−1 that is lower than 100 mPa·s, preferably lower than 90 mPa·s, more preferably lower than 80 mPa·s and most preferably lower than 70 mPa·s and preferably at least 30 mPa·s, more preferably at least 40 mPa·s, even more preferably at least 50 mPa·s and
- a creep compliance Jmax measured at 23° C. after 300 seconds using a creep stress of 1.0 Pa of lower than 250 Pa−1, preferably lower than 150 Pa−1 and even more preferably lower than 50 Pa−1.
A non-aqueous thixotropic resin composition, comprising a resin and a thixotropy agent comprising polyurea particles characterised in that the composition has
- a) a high-shear viscosity HSV measured at 23° C. at a shear rate of 1000±50 s−1 that is lower than 100 mPa·s, preferably lower than 90 mPa·s, more preferably lower than 80 mPa·s and even more preferably lower than 70 mPa·s and preferably at least 30 mPa·s, more preferably at least 40 mPa·s, even more preferably at least 50 mPa·s and
- b) a creep compliance Jmax measured at 23° C. after 300 seconds using a creep stress of 1.0 Pa of lower than 250 Pa−1, preferably lower than 150 Pa−1 and even more preferably lower than 50 Pa−1,
- c) an amount of the polyurea particles between 0.4 and 2.5 cwt %, preferably between 0.5 and 2.0 cwt %, more preferably between 0.6 and 1.8 cwt % or most preferably between 0.7 and 1.7 cwt %,
- which non-aqueous thixotropic resin composition preferably is a clear-coat composition not comprising pigments.
Dependencies are inferred from the claim text.