Nanocrystalline soft magnetic material
AssigneeDaido Steel Co., Ltd.
InventorYuya TOMITA
Life of this patent
Estimating the term…
Abstract
The present invention relates to a nanocrystalline soft magnetic material in which Fe—Si crystal grains having an average grain diameter of 20 nm or less are dispersed in an amorphous matrix phase, the nanocrystalline soft magnetic material including: an alloy composition including, in terms of at %, Si: 14.0% to 18.0%, B: 6.0% to 10.0%, Nb: 1.0% to 5.0%, Cu: 0.5% to 1.5%, and C: more than 0.40% to 1.0%, with the balance being Fe and unavoidable impurities, in which the nanocrystalline soft magnetic material has a coercive force Hc of 1.0 A/m or less and a saturation magnetic flux density Bs of larger than 1.0 T.
Claims12
A nanocrystalline soft magnetic material in which Fe—Si crystal grains having an average grain diameter of 20 nm or less are dispersed in an amorphous matrix phase, the nanocrystalline soft magnetic material comprising:
- an alloy composition comprising, in terms of at %,
- Si:
- 14.0% to 18.0%,
- B:
- 6.0% to 10.0%,
- Nb:
- 1.0% to 5.0%,
- Cu:
- 0.5% to 1.5%, and
- C:
- more than 0.40% to 1.0%,
- with the balance being Fe and unavoidable impurities, wherein
- the nanocrystalline soft magnetic material has a coercive force Hc of 1.0 A/m or less and a saturation magnetic flux density Bs of larger than 1.0 T.
A nanocrystalline soft magnetic material in which Fe—Si crystal grains having an average grain diameter of 20 nm or less are dispersed in an amorphous matrix phase, the nanocrystalline soft magnetic material comprising:
- an alloy composition comprising, in terms of at %,
- Si:
- 14.0% to 18.0%,
- B:
- 6.0% to 10.0%,
- Nb:
- 1.0% to 5.0%,
- Cu:
- 0.5% to 1.5%, and
- at least one kind selected from the group consisting of C, P, and S provided that at least P or S is contained such that 0.01≤[C]+[P]+2[S]≤1.00 is satisfied, where [M]% is at % of an element M,
- with the balance being Fe and unavoidable impurities, wherein
- the nanocrystalline soft magnetic material has a coercive force Hc of 1.0 A/m or less and a saturation magnetic flux density Bs of larger than 1.0 T.