A binder composition free of phenol compound
OwnerSanna VALKONENinventor
Life of this patent
Estimating the term…
Abstract
A method for producing a binder composition without using a compound selected from the class of phenols, is disclosed. The method comprises: (i) heating an aqueous composition comprising lignin and lignin oligomer in the presence of a catalyst at a temperature of 50-95° ° C. for 0.25-5 hours; (ii) mixing a cross-linking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and cross-linking agent until a binder composition with a predetermined viscosity value is formed; wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.
Claims13
A method for producing a binder composition without using a compound selected from the class of phenols, wherein the method comprises:
- (i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours;
- and
- (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed,
- wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.
A binder composition obtainable by a method comprising:
- (i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours;
- and
- (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed,
- wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8.
A product comprising:
- a binder composition obtained by the method comprising (i) heating an aqueous composition comprising lignin having a weight average molecular weight (Mw) of 2700-9000 g/mol and lignin oligomer having a weight average molecular weight (Mw) of 800-2500 g/mol in the presence of a catalyst at a temperature of 50-95° C. for 0.25-5 hours, and (ii) mixing a crosslinking agent with the aqueous composition from (i) and heating the same at a temperature of 60-95° C. for polymerizing lignin, lignin oligomers, and crosslinking agent until a binder composition with a predetermined viscosity value is formed, wherein the molar ratio of crosslinking agent to lignin and lignin oligomer is 0.5-1.8,
- wherein the product has one or more of the following properties:
- the amount of formaldehyde emissions being 0.01-0.5 mg/l, when measured by desiccator method EN ISO 12460-4,
- the amount of formaldehyde emissions being 0.01-0.40 mg/m2*h, when measured by gas analysis EN ISO 12460-3, and
- fulfilling the minimum bonding class 1-4, when measured by bonding quality test method EN 314-1 & EN314-2.
Dependencies are inferred from the claim text.