Back to results
US 2024/0186490 A1Published application
Battery positive electrode material, preparation method therefor, and application thereof
AssigneeBYD Company Limited
InventorsBin CHENG, Yi PAN, Minghao ZHUANG, Yuzhen YE, Ruoyi DENG
Life of this patent
Estimating the term…
Abstract
A battery positive electrode material includes a core and a first shell layer arranged on a surface of the core. The core includes LiMnxFe1-xPO4. The first shell layer includes LiMnyFe1-yPO4, where 0<x≤0.4, and 0.6≤y≤0.9. The battery positive electrode material has a multi-layer distribution structure. A preparation method and use of the battery positive electrode material are further provided.
Claims20
A battery positive electrode material, comprising:
- a core and a first shell layer arranged on a surface of the core, the core comprising LiMnxFe1-xPO4, and the first shell layer comprising LiMnyFe1-yPO4, wherein 0<x≤0.4, and 0.6≤y≤0.9.
A method for preparing a battery positive electrode material, comprising:
- subjecting a lithium source, an iron source, a manganese source, a phosphorus source, and a solvent to a first reaction in a reactor to obtain a core, the core comprising LiMnxFe1-xPO4, wherein 0<x≤0.4, a temperature of the first reaction being between 375° C. and 500° C., and a pressure of the first reaction being greater than or equal to 23 MPa;
- subjecting a lithium source, an iron source, a manganese source, a phosphorus source, a solvent, and the core to a second reaction in a reactor to coat a first shell layer on a surface of the core to obtain the core with the first shell layer, the first shell layer comprising LiMnyFe1-yPO4, wherein 0.6≤y≤0.9, a temperature of the second reaction being between 375° C. and 500° C., and a pressure of the second reaction being greater than or equal to 23 Mpa;
- and
- calcining the core with the first shell layer at between 500° C. and 800° C. to obtain the battery positive electrode material.
1 more element
Dependencies are inferred from the claim text.