Method for producing grain-oriented electrical steel sheet
AssigneeJfe Steel Corporation
InventorsRyosuke Tani, Takeshi Imamura, Shigehiro Takajo, Hiroi Yamaguchi
Life of this patent
Estimating the term…
Loading patent…
AssigneeJfe Steel Corporation
InventorsRyosuke Tani, Takeshi Imamura, Shigehiro Takajo, Hiroi Yamaguchi
Estimating the term…
A method for producing a grain-oriented electrical steel sheet comprises heating a steel material containing a certain composition to a temperature in a range of 1150 to 1250° C.; performing hot rolling, hot-band annealing, and cold rolling on the material to obtain a cold-rolled sheet with a final thickness; performing decarburization annealing also serving as primary recrystallization annealing on the cold-rolled sheet; subsequently applying an annealing separator to a surface of the steel sheet; and performing finishing annealing followed by applying an insulation coating. In the method, rapid heating is conducted from 500 and 700° C. in a heating process of the decarburization annealing at a rate of 100 to 1000° C./s while gradual heating is conducted from 800 to 900° C. in a heating process of the finishing annealing at a heating rate of 0.5 to 4.0° C./hr for at least 10 hours.
A method for producing a grain-oriented electrical steel sheet comprising
Dependencies are inferred from the claim text.