Back to results
US 2024/0140813 A1Published application
Boehmite and method for producing same
AssigneeSumitomo Chemical Company, Limited
InventorsTeppei KAJINO, Yoshitaka KAWAKAMI, Kohei SOGABE
Life of this patent
Estimating the term…
Abstract
Disclosed is boehmite having a ratio of a micropore volume to a mesopore volume of 0.50 or more and a loose bulk density of 0.30 g/mL or more. The loose bulk density is preferably 0.70 g/mL or more.
Claims5
Boehmite having a ratio of a micropore volume to a mesopore volume of 0.50 or more and a loose bulk density of 0.30 g/mL or more.
A method for producing boehmite, comprising:
- a first hydrolysis step of adding a first hydrolysis liquid containing an aqueous alcohol solution having a water concentration of 5% by weight or more and 80% by weight or less to a solution containing aluminum alkoxide so that a molar ratio of water to aluminum alkoxide falls within a range of 1.5 or more and 2.0 or less to perform hydrolysis;
- a second hydrolysis step of adding a second hydrolysis liquid containing water or an aqueous alcohol solution to the resulting solution so that the molar ratio of water to aluminum alkoxide falls within a range of 1.0 or more and 7.0 or less to perform hydrolysis;
- a step of removing water and alcohol from the resulting solution to recover a boehmite powder;
- and
- a step of stirring and drying the boehmite powder at a drying temperature of 80° C. or higher and 110° C. or lower while humidifying the boehmite powder so that a humidity is 80% or more and 100% or less,
- wherein at least one of the first hydrolysis liquid and the second hydrolysis liquid contains 0.05 parts by weight or more and 10 parts by weight or less of an organic carboxylic acid with respect to the boehmite obtained after drying.
3 more elements
Dependencies are inferred from the claim text.