Alkali doped optical fiber with reduced attenuation
AssigneeCorning Incorporated
InventorsSushmit Sunil Kumar Goyal, Craig Daniel Nie, Pushkar Tandon
Life of this patent
Estimating the term…
Loading patent…
AssigneeCorning Incorporated
InventorsSushmit Sunil Kumar Goyal, Craig Daniel Nie, Pushkar Tandon
Estimating the term…
A method of manufacturing an optical fiber, the method includes drawing a first optical fiber preform at a first draw tension to produce a first alkali doped optical fiber and drawing the first optical fiber preform at a second draw tension to produce a second alkali doped optical fiber, measuring the attenuation of the first alkali doped optical fiber and the second alkali doped optical fiber such that the second alkali doped optical fiber has a lower attenuation. Additionally, the method includes setting the draw tension to the second draw tension and drawing a second optical fiber preform at the second draw tension to produce a third alkali doped optical fiber. The third alkali-doped optical fiber has an attenuation at 850 nm of about 1.50 dB/km or less and an attenuation at 1550 nm of about 0.155 dB/km or less.
A method of manufacturing an optical fiber, the method comprising:
A method of manufacturing an optical fiber, the method comprising:
A method of manufacturing an optical fiber, the method comprising:
Dependencies are inferred from the claim text.