Weld joint and production method therefor
AssigneesJfe Steel Corporation, Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsAtsushi TAKADA, Peng HAN, Masamichi SUZUKI
Life of this patent
Estimating the term…
Loading patent…
AssigneesJfe Steel Corporation, Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsAtsushi TAKADA, Peng HAN, Masamichi SUZUKI
Estimating the term…
Provided is a weld joint having high strength and excellent hot crack resistance and low-temperature toughness. High Ni steel plates containing 6.5 mass % to 10.0 mass % of Ni are welded to form a weld metal to obtain a weld joint. The weld metal has a chemical composition containing Mn: 13.0% to 25.0%, Cr: 3.8% or less, Ni: 1.0% to 12.0%, Mo: 0.1% to 5.0%, N: % or less, and O: 0.100% or less, and the strength of the weld metal is adjusted so that the yield strength BYS of each steel plate and the 0.2% proof stress WPS of the weld metal satisfy [WPS]≤[BYS]−100 MPa (1) and the tensile strength BTS of the steel plate and the tensile strength WTS of the weld metal satisfy [WTS]≤[BTS]+100 MPa (2).
A weld joint comprising steel plates and a weld metal, the weld joint formed by welding the steel plates through the weld metal,
A production method for a weld joint excellent in low-temperature toughness, comprising:
Dependencies are inferred from the claim text.