Laminate and method for producing same
AssigneeKaneka Corporation
InventorsHanako Hasebe, Haruki Koyama, Yukihiro Shimamoto
Life of this patent
Estimating the term…
Abstract
A laminate having excellent moldability and including an acrylic-based resin film is provided. A method for producing a laminate having a specific crack elongation, includes a step (A) of forming, on at least one side of a specific acrylic-based resin film, a hard coat layer that contains a urethane acrylate resin, and a step (B) of forming, on the hard coat layer obtained in the step (A), a low refractive index layer that contains, in an amount of not less than 40%, hollow fine silica particles having a particle size of less than 100 nm and that contains an acrylate-based resin.
Claims33
A method for producing a laminate, comprising:
- a hard coat layer forming step (A1) of irradiating a resin layer, containing a urethane acrylate resin, that has been applied to at least one side of an acrylic-based resin film, with an active energy ray to cure the resin layer containing the urethane acrylate resin thereby obtaining a hard coat layer;
- and
- a low refractive index layer forming step (B1) of applying, an acrylate-based resin containing hollow fine silica particles having a particle size of less than 100 nm in an amount of not less than 40%, onto the hard coat layer obtained in the step (A1) and irradiating a resultant resin layer that contains the acrylate-based resin with an active energy ray to cure the resin layer that contains the acrylate-based resin,
- wherein
- the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C., and
- the laminate has a crack elongation of not less than 80% at 120° C.
A method for producing a laminate, comprising:
- a hard coat layer forming step (A1) of irradiating a resin layer, containing urethane acrylate resin, that has been applied to at least one side of an acrylic-based resin film, with an active energy ray to cure the resin layer containing the urethane acrylate resin thereby obtaining a hard coat layer;
- wherein
- the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C., and the hard coat layer contains the urethane acrylate resin, and
- the laminate has a crack elongation of not less than 80% at 120° C.
A laminate comprising:
- an acrylic-based resin film;
- and
- a hard coat layer that is laminated on at least one side of the acrylic-based resin film,
- wherein
- the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
- the hard coat layer contains a urethane acrylate resin, and
- the laminate has a pencil hardness of not less than H, and a crack elongation of not less than 80% at 120° C.
A method for producing a laminate, comprising:
- a hard coat layer forming step (A2) of irradiating a resin layer, containing a urethane acrylate resin and particles, that has been applied to at least one side of an acrylic-based resin film with an active energy ray to cure the resin layer containing the urethane acrylate resin and the particles, thereby obtaining a hard coat layer;
- wherein
- the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
- the particles are contained in an amount of 2.0% by weight to 5.0% by weight with respect to the hard coat layer that has been cured,
- d≤r is satisfied, where r (μm) is an average dispersed particle size of the particles, and d (μm) is a thickness of the hard coat layer,
- the laminate has a pencil hardness of not less than H, a haze of not less than 3%, and a crack elongation of not less than 170% at 120° C., and
- a laminated film obtained by laminating, on the acrylic-based resin film, a resin layer not containing the particles has a crack elongation of not less than 80% at 120° C.
A laminate comprising:
- an acrylic-based resin film;
- and
- a hard coat layer that is laminated on at least one side of the acrylic-based resin film, wherein
- the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
- the hard coat layer contains a urethane acrylate resin and particles,
- d≤r is satisfied, where r (μm) is an average dispersed particle size of the particles, and d (μm) is a thickness of the hard coat layer,
- the laminate has a pencil hardness of not less than H and a haze of not less than 3%, and
- a laminated film obtained by laminating, on the acrylic-based resin film, a resin layer not containing the particles has a crack elongation of not less than 80% at 120° C.
Dependencies are inferred from the claim text.