Method for producing a welded steel blank and associated welded blank
AssigneeArcelorMittal
InventorsCristian ALVAREZ, Thierry LIZON, Maria POIRIER
Life of this patent
Estimating the term…
Loading patent…
AssigneeArcelorMittal
InventorsCristian ALVAREZ, Thierry LIZON, Maria POIRIER
Estimating the term…
A method for producing a welded blank (1) includes providing two precoated sheets (2), butt welding the precoated sheets (2) using a filler wire. The precoating (5) entirely covers at least one face (4) of each sheet (2) at the time of butt welding. The filler wire (20) has a carbon content between 0.01 wt. % and 0.45 wt. %. The composition of the filler wire (20) and the proportion of filler wire (20) added to the weld pool is chosen such that the weld joint (22) has (a) a quenching factor FTWJ: FTWJ−0.9FTBM≥0, where FTBM is a quenching factor of the least hardenable substrate (3), and FTWJ and FTBM are determined: FT=128+1553×C+55×Mn+267×Si+49×Ni+5×Cr−79×Al−2×Ni2−1532×C2−5×Mn2−127×Si2−40×C×Ni−4×Ni×Mn, and (b) a carbon content CWJ<0.15 wt. % or, if CWJ≥0.15 wt. %, a softening factor FAWJ such that FAWJ>5000, where FA=10291+4384.1×Mo+3676.9Si−522.64×Al−2221.2×Cr−118.11×Ni−1565.1×C−246.67×Mn.
A method for producing a welded steel blank comprising the successive steps of:
A welded steel blank comprising:
A welded, hot press-formed and cooled steel part comprising:
Dependencies are inferred from the claim text.