Water-containing glass-based articles with high indentation cracking threshold
AssigneeCorning Incorporated
InventorsTimothy Michael Gross, Georgiy M. Guryanov
Life of this patent
Estimating the term…
Abstract
Glass-based articles that include a hydrogen-containing layer extending from the surface of the article to a depth of layer. The hydrogen-containing layer includes a hydrogen concentration that decreases from a maximum hydrogen concentration to the depth of layer. The glass-based articles exhibit a high Vickers indentation cracking threshold. Glass compositions that are selected to promote the formation of the hydrogen-containing layer and methods of forming the glass-based article are also provided.
Claims20
A glass article strengthened by steam treatment, comprising:
- a surface of the glass article;
- a hydrogen-containing layer extending from the surface into the glass article to a depth of layer, wherein the depth of layer refers to a first depth below the surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
- and
- a compressive stress layer from hydrogen species, the compressive stress layer extending from the surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile;
- wherein the depth of layer is greater than 5 μm from the surface;
- and
- wherein the compressive stress layer comprises compressive stress of at least 100 MPa.
A glass article, comprising:
- a first surface, a second surface, and a thickness that extends therebetween, wherein the article is shaped as a sheet such that the first and second surfaces are opposing major surfaces thereof;
- a hydrogen-containing layer extending from the first surface into the glass article to a depth of layer, wherein the depth of layer refers to a first depth below the first surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
- and
- a compressive stress layer from hydrogen species, the compressive stress layer extending from the first surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile;
- wherein the depth of layer is greater than or equal to 20 μm;
- and
- wherein the compressive stress layer comprises compressive stress of at least 100 MPa.
A glass article, comprising:
- a first surface, a second surface, and a thickness that extends therebetween;
- a first hydrogen-containing layer extending from the first surface into the glass article to a first depth of layer, wherein the first depth of layer refers to a first depth below the first surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
- a second hydrogen containing layer extending from the second surface into the article to a second depth of layer, wherein the second depth of layer refers to a first depth below the second surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
- a region between the first depth of layer and the second depth of layer, wherein hydrogen concentration is substantially constant between the first depth of layer and the second depth of layer;
- a compressive stress layer from hydrogen species, the compressive stress layer extending from the first surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile;
- and
- a tensile stress region, whereby forces within the glass article are balanced;
- wherein the first depth of layer is greater than 0.005 times the thickness and less than or equal to 0.205 times the thickness, wherein the thickness is less than or equal to 2 mm;
- wherein the compressive stress layer comprises compressive stress of at least 100 MPa;
- wherein at least a portion of the compressive stress layer is free of larger alkali ions exchanged into the glass for smaller alkali ions, corresponding to traditional ion-exchange strengthening;
- and
- where the tensile stress region comprises a maximum central tension greater than or equal to 10 MPa.
Dependencies are inferred from the claim text.