Oxidative stability test methods for chemically recycled plastic feedstocks
AssigneeEcolab USA Inc.
InventorsAshish DHAWAN, Carter M. SILVERNAIL, Emily Rebecca WOOD, Kameswara VYAKARANAM, Daniel Robert DREYER, Karina EURESTE
Life of this patent
Estimating the term…
Abstract
The present disclosure relates to various testing methods that can be applied to oils, such as pyrolysis oils. Different testing methods can be used to determine the oxidative stability of an oil. The testing methods may also be used to differentiate between various oils and to determine the effectiveness of various antioxidants on the oxidative stability of an oil.
Claims26
A method of determining the oxidative stability of a pyrolysis oil, comprising:
- heating a sample of the pyrolysis oil to a temperature from about 50° C. to about 220° C.,
- passing a stream of air through the sample of pyrolysis oil,
- forming a volatile reaction product,
- transporting the volatile reaction product into a measurement solution comprising deionized water, and
- measuring an electrical conductivity of the measurement solution.
A method of determining the ability of an antioxidant to stabilize a pyrolysis oil, comprising:
- heating a first sample comprising the pyrolysis oil to a first temperature from about 50° C. to about 220° C.,
- passing a first stream of air through the sample of pyrolysis oil,
- forming a first volatile reaction product,
- transporting the first volatile reaction product into a first measurement solution comprising deionized water,
- measuring an electrical conductivity of the first measurement solution for a first period of time until an increase in conductivity is detected,
- adding the antioxidant to a second sample of the pyrolysis oil,
- heating the second sample to the first temperature,
- passing a second stream of air through the second sample,
- forming a second volatile reaction product,
- transporting the second volatile reaction product into a second measurement solution comprising deionized water,
- measuring an electrical conductivity of the second measurement solution for a second period of time until an increase in conductivity is detected, and
- comparing the first period of time to the second period of time.
A method of determining the oxidative stability of a pyrolysis oil, comprising:
- introducing a sample of the pyrolysis oil into a sample chamber,
- pressurizing the sample chamber to a pressure from about 200 kPa to about 700 kPa with O2,
- heating the sample of the pyrolysis oil to a temperature from about 100° C. to about 180° C.,
- monitoring a pressure within the sample chamber, and
- determining a time at which a decrease in the pressure within the sample chamber is detected.
A method of determining the oxidative stability of a pyrolysis oil, comprising:
- introducing a sample of the pyrolysis oil into a sample chamber,
- pressurizing the sample chamber to a pressure from about 100 psi to about 1,000 psi with O2,
- heating the sample of the pyrolysis oil to a temperature of about 90° C. to about 250° C.,
- holding the sample at the pressure and the temperature until an exothermic reaction is detected, and
- determining a period of time from a beginning of the pressurizing step to a time when the exothermic reaction is detected.