Back to results
US 2023/0278874 A1Published application
Carbonized upgraded coal, graphite, and methods of making the same
OwnerAlexander Azenkeng, Jason D. Laumbinventors
Life of this patent
Estimating the term…
Abstract
A method of forming graphite includes carbonizing an upgraded coal, to form a carbonized upgraded coal. The method also includes graphitizing the carbonized upgraded coal, to form the graphite.
Claims20
A method of carbonizing an upgraded coal, the method comprising:
- heating the upgraded coal in an inert environment, to form a carbonized upgraded coal.
A method of forming graphite, the method comprising:
- cleaning coal to form a cleaned coal residue;
- at least one of
- reacting the cleaned coal residue with an oxidizable inorganic metallic agent, and
- reacting the cleaned coal residue with a reducing agent,
- to form an upgraded coal;
- heating the upgraded coal to a temperature of 500° C. to 2,000° C. in an inert environment, to form a carbonized upgraded coal;
- controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 0 wt% to <7 wt%;
- and
- heating the carbonized upgraded coal to a graphitization temperature in the range of 2500° C. to 3500° C. for a graphitization duration of 10 min to 10 h, to form the graphite, wherein in the graphite a weight ratio of croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels to graphulerenite is equal to or greater than 100:1.
6 more elements
A method of forming graphite, the method comprising:
- cleaning coal to form a cleaned coal residue;
- at least one of
- reacting the cleaned coal residue with an oxidizable inorganic metallic agent, and
- reacting the cleaned coal residue with a reducing agent,
- to form an upgraded coal;
- heating the upgraded coal to a temperature of 500° C. to 2,000° C. in an inert environment, to form a carbonized upgraded coal;
- controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 5.6 wt% to 20 wt%;
- and
- heating the carbonized upgraded coal to a graphitization temperature in the range of 2500° C. to 3500° C. for a graphitization duration of 10 min to 10 h, to form the graphite, wherein in the graphite a weight ratio of graphulerenite to croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels is equal to or greater than 100:1.
6 more elements