Semiconductor device and method for manufacturing the semiconductor device
AssigneeSemiconductor Energy Laboratory Co., Ltd.
InventorsShunpei YAMAZAKI, Tetsuya KAKEHATA, Yuji EGI, Yasuhiro JINBO, Yujiro SAKURADA
Life of this patent
Estimating the term…
Abstract
A semiconductor device having favorable electrical characteristics is provided. A metal oxide is formed over a substrate by the steps of: introducing a first precursor into a chamber in which the substrate is provided; introducing a first oxidizer after the introduction of the first precursor; introducing a second precursor after the introduction of the first oxidizer; and introducing a second oxidizer after the introduction of the second precursor.
Claims16
(canceled)
A method for manufacturing a metal oxide, comprising:
- a first step of introducing a precursor;
- a second step of performing a first evacuation after the introduction of the precursor;
- a third step of introducing an oxidizer after the first evacuation;
- and
- a fourth step of performing a second evacuation after the introduction of the oxidizer.
A method for manufacturing a metal oxide, comprising:
- a first step of introducing a precursor;
- a second step of performing a first evacuation after the introduction of the precursor;
- a third step of introducing an oxidizer after the first evacuation;
- and
- a fourth step of performing a second evacuation after the introduction of the oxidizer,
- wherein the precursor contains chlorine, and
- wherein the metal oxide comprises a crystal structure in which a c-axis of a crystal is aligned perpendicularly to a deposition surface.
A method for manufacturing a metal oxide, comprising:
- a first step of introducing a precursor;
- a second step of performing a first evacuation after the introduction of the precursor;
- a third step of introducing an oxidizer after the first evacuation;
- and
- a fourth step of performing a second evacuation after the introduction of the oxidizer,
- wherein the precursor contains chlorine,
- wherein the metal oxide comprises a crystal structure in which a c-axis of a crystal is aligned perpendicularly to a deposition surface, and
- wherein the first step to the fourth step are performed at a temperature higher than or equal to 200° C. and lower than or equal to 400° C.
Dependencies are inferred from the claim text.