Process for manufacturing high strength steel
AssigneeUnited States Steel Corporation
InventorMatthew J. Merwin
Life of this patent
Estimating the term…
Abstract
A method of making high strength steel sheet with a tensile strength of 800 to 1000 MPa and a hole expansion ratio of at least 50%, comprising the steps of reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3; hot rolling the slab to final desired thickness; cooling the steel sheet at a rate of 50° C. per second to a temperature less than 400° C.; and winding the steel sheet into a coil.
Claims19
A method of making high strength steel sheet with a tensile strength of 800 to 1100 MPa and a hole expansion ratio of at least 50%, comprising the steps of:
- reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3;
- hot rolling the slab to final desired thickness;
- cooling the steel sheet at a rate of 50° C. per second to a temperature less than 400° C.;
- and
- winding the steel sheet into a coil.
A method of making high strength steel sheet having a tensile strength of approximately 800 MPa and a composition of 0.06 weight percent of Carbon, 1.0 weight percent of Mn and 0.1 weight percent of Si, 0.03 weight percent of Ti and 0.0020 weight percent of boron, comprising the steps of:
- reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3;
- than 400° C.;
- and
- hot rolling the slab to final desired thickness;
- cooling the steel sheet at a rate of 50° C. per second to a temperature less winding the steel sheet into a coil.
A method of making high strength steel sheet a tensile strength of approximately 1000 MPa and a composition 0.06 weight percent of C, 1.0 weight percent of Mn, 0.1 weight percent of Si, 0.03 weight percent of Ti and 0.0020 weight percent of B, comprising the steps of:
- slab, above Ar3;
- than 400° C.;
- and
- reheating a previously cast slab, or retaining the heat from a directly cast hot rolling the slab to final desired thickness;
- cooling the steel sheet at a rate of 50° C. per second to a temperature less winding the steel sheet into a coil.
Dependencies are inferred from the claim text.