Hot rolled steel sheet
AssigneeNippon Steel Corporation
InventorsTakeshi TOYODA, Eisaku SAKURADA
Life of this patent
Estimating the term…
Abstract
Provided is a hot rolled steel sheet having a tensile strength of 780 MPa or more, a sheet thickness of 1.2 to 4.0 mm, and a sheet width of 750 mm or more, and satisfying -15≤(λW 1 +λW2)/2-λC ≤15 (where λW1 and λW2 respectively indicate hole expansion ratios (%) at ⅛ positions of the sheet width from one end of the hot rolled steel sheet in a sheet width direction perpendicular to a rolling direction and the other end at an opposite side, and λC indicates a hole expansion ratio (%) of a sheet width center part).
Claims8
1-9. (canceled)
A hot rolled steel sheet having a tensile strength of 980 MPa or more, a sheet thickness of 1.2 to 4.0 mm, and a sheet width of 750 mm or more, and satisfying the following formula 1:
- -
- 15
- ≤
- λ
- W1
- +
- λ
- W2
- /
- 2
- -
- λ
- C
- ≤
- 15
- formula 1
- where λW1 and λW2 respectively indicate hole expansion ratios (%) at ⅛ positions of the sheet width from one end of the hot rolled steel sheet in a sheet width direction perpendicular to a rolling direction and the other end at an opposite side, λC indicates a hole expansion ratio (%) of a sheet width center part, and λW1, λW2, and λC are respectively 40% or more,
- wherein the hot rolled steel sheet has a chemical composition comprising, by mass%,
- C:
- 0.01 to 0.50%,
- Si:
- 0.01 to 3.50%,
- Mn:
- 0.20 to 3.00%,
- P:
- 0.100% or less,
- S:
- 0.0200% or less,
- N:
- 0.0100% or less,
- Al:
- 0.001 to 1.000%,
- Cu:
- 0 to 1.00%,
- Ni:
- 0 to 0.50%,
- Cr:
- 0 to 2.00%,
- Mo:
- 0 to 3.00%,
- W:
- 0 to 0.10%,
- Nb:
- 0 to 0.060%,
- V:
- 0 to 1.00%,
- Ti:
- 0 to 0.20%,
- B:
- 0 to 0.0040%,
- O:
- 0 to 0.020%,
- Ta:
- 0 to 0.10%,
- Co:
- 0 to 3.00%,
- Sn:
- 0 to 1.00%,
- Sb:
- 0 to 0.50%,
- As:
- 0 to 0.050%,
- Mg:
- 0 to 0.050%,
- Zr:
- 0 to 0.050%,
- Ca:
- 0 to 0.0500%,
- REM:
- 0 to 0.0500%, and
- balance:
- Fe and impurities.
Dependencies are inferred from the claim text.