In various aspects, the present disclosure pertains to thermoformed webs that comprise polymer films having one or more thermoformed cavities contained therein, the polymer films comprising a polymer blend of amorphous polyethylene terephthalate (APET), polyethylene furanoate (PEF), and a copolyester that comprises (a) dicarboxylic acid residues (e.g., dicarboxylic acid residues that comprise terephthalic acid residues and, optionally, one or more additional dicarboxylic acid residues) and (b) diol residues (e.g., diol residues comprising ethylene glycol residues and, optionally, one or more additional diol monomer residues). Other aspects of the disclosure pertain to methods of forming such thermoformed webs, packaged products comprising such thermoformed webs, and methods of recycling such thermoformed webs.
A thermoformed web comprising a polymer film and having one or more thermoformed cavities contained therein, wherein the polymer film comprises a polymer blend of 0 wt % to 95 wt % of amorphous polyethylene terephthalate (APET), 0 wt % to 95% polyethylene furanoate (PEF), and 5 wt % to 50 wt % of a copolyester that comprises (a) dicarboxylic acid residues comprising polyethylene terephthalate residues and (b) diol residues comprising (i) ethylene glycol residues and (ii) one or more additional diol monomer residues selected from neopentyl glycol residues, 1,4-cyclohexanedimethanol residues, or diethylene glycol residues, wherein the polymer film has a maximum shrinkage during processing of 8% or less.
A thermoformed web comprising a polymeric film and having one or more thermoformed cavities contained therein, wherein the polymer film comprises a polymer blend of amorphous polyethylene terephthalate (APET), polyethylene furanoate (PEF), and a copolyester that comprises (a) dicarboxylic acid residues comprising polyethylene terephthalate residues and (b) diol residues comprising (i) ethylene glycol residues and (ii) one or more additional diol monomer residues, wherein the polymer film has a crystallization time of at least 2 minutes at an isothermal crystallization temperature of 120° C. as measured by DSC, wherein the polymer film has a maximum shrinkage during processing of 8% or less.