Abstract
The disclosure relates to seamless manufacturing processes for 3-dimensional waterproof and breathable porous polymer membranes by spraying, dip-coating or painting a substrate with a dispersion having polymer, coated or non-coated particles and diluent and removing the particles by dissolution thus creating porosity after the 3D coating/shaping. The disclosure further relates to dispersions to obtain such membranes, to polymer membranes obtained, to shaped articles containing such membranes; to the use of such membranes, shaped articles and intermediates.
Claims16
A method of manufacturing a polymer membrane:
- said polymer membrane
- is 3-dimensional and seamless;
- is either a membrane attached to a substrate, or is a free-standing membrane;
- is porous and having a pore size of 500-2,000 nm,
- said method comprising the steps of:
- a. providing a dispersion having a viscosity of 400-1500 mPas at 25° C. and 200 rpm, the dispersion comprising
- one or more diluents in an amount of at least 40 wt.%;
- one or more polymers dissolved therein;
- one or more coated or non-coated particles dispersed therein;
- optionally one or more additives dissolved therein;
- and
- optionally one or more dyes dispersed therein, and whereby the coated particles
- are pre-manufactured;
- are selected from the group consisting of organic salts, metal salts, metal oxides and combinations thereof, or organic crystals;
- the coating material of said coated particles is selected from the group of poly maleic anhydrides, carboxylic acids, aryl-alkoxy-silanes alkyl-aryl-alkoxy-silanes and alkyl-alkoxy-silanes;
- and
- have a particle size in the range of 5-15,000 nm, preferably 2000-8000 nm, and whereby the non-coated particles
- are selected from the group consisting of organic salts, metal salts, metal oxides and combinations thereof, or organic crystals;
- have a particle size in the range of 5 - 15,000 nm, preferably 2000-8000 nm;
- b. coating a 3-dimensional substrate with said dispersion, thus obtaining a layer partly or fully covering said substrate;
- c. subjecting the obtained material to a drying step, thus obtaining a dried material;
- d. optionally repeating steps (b) and (c), thus obtaining a multi-coated material;
- e. optionally subjecting the thus obtained material to a polymerisation or cross-linking step;
- f. removing said one or more particles by a dissolution step, thus obtaining a porous polymer membrane attached to a substrate;
- and
- g. optionally removing the obtained polymer porous membrane from said substrate without destruction of the 3-dimensional shape, thus obtaining a free-standing 3D membrane;
- and wherein said 3D structure comprise three distinctive coordinates y, z and x and thereby excludes 2D structures and bent 2D structures;
- and
- wherein said polymer has a solubility in a solvent of at least 1 g/l, preferably 10 g/l.