Back to results
US 2023/0211333 A1Published application
Regenerating the catalytic activity of a spent catalyst
AssigneeTopsoe A/S
InventorJens Henrik HYLDTOFT
Life of this patent
Estimating the term…
Abstract
The invention relates to a method of regenerating the catalytic activity of a spent catalyst comprising nickel on a refractory oxide support, said method comprising the steps of contacting the spent catalyst with a nitric acid solution, heat-treating the spent catalyst, calcining and reducing the catalyst.
Claims15
A method of regenerating the catalytic activity of a spent catalyst comprising nickel, said spent catalyst being:
- (a) a spent steam reforming catalyst in which the nickel content is 5-20 wt % Ni and the support is an oxide comprising aluminium, zirconium, magnesium, calcium, lanthanum, yttrium, and/or cerium, and wherein the spent catalyst is provided in the form of tablets or pellets, or
- (b) a spent steam reforming catalyst in which the nickel content is 5-20 wt % Ni, said spent steam reforming catalyst being a structured catalyst comprising a macroscopic structure, wherein said macroscopic structure is formed by a metallic material and at least partly support a refractory oxide support;
- said method comprising only the steps of:
- i) contacting the spent catalyst with a nitric acid solution, in which the nitric acid solution is at least 60 wt % HNO3, and adding one or more organic acids;
- ii) heat-treating the spent catalyst at a suitable temperature for reacting nickel with nitric acid, said suitable temperature being in the range 50-100° C., and subsequently drying the catalyst at 100-125° C.;
- iii) calcining and reducing the catalyst, in which the calcining step is conducted in air at 500-1300° C. for 1-4 hours, and the reducing step is conducted in the presence of hydrogen at 400-600° C. for 2-4 hours.
3 more elements
Dependencies are inferred from the claim text.