US 2023/0193092 A1Published application
Blended furnish with improved performance and methods of making and using the same
AssigneeArclin USA LLC
InventorsSamuel W. LONBERG, Matthew E. TUCKER
Life of this patent
Estimating the term…
Abstract
A blended furnish with improved performance characteristics while reducing environmental impact, when applied to a substrate and methods of making and using blended furnish are provided. A composite product using a blended furnish is also provided.
Claims20
A blended furnish, comprising:
- a urea-formaldehyde (UF) resin or a melamine-urea-formaldehyde (MUF) resin;
- a lignosulfonate or a kraft lignin;
- an alkaline compound;
- optionally an additive;
- and
- a plurality of substrates,
- wherein the blended furnish has a buffer capacity of 2-200 mL of 0.1 N HCl by the Acid Titration Value (ATV) Method using 20 grams of blended furnish for a period of time up to 20 days.
4 more elements
A method for preparing a blended furnish, comprising:
- adding a plurality of substrates;
- mixing a urea-formaldehyde (UF) resin or a melamine-urea-formaldehyde (MUF) resin optionally with an amine and water at a pH of 5-11, preferably 6-10;
- optionally adding one or more additives;
- adding a lignosulfonate salt or a kraft lignin;
- optionally adding one or more additives to form the blended furnish,
- wherein the blended furnish has a buffer capacity of 2-200 mL of 0.1 N HCl by the Acid Titration Value (ATV) Method using 20 grams of blended furnish for a period of time up to 20 days.
3 more elements
A method for preparing a blended furnish, comprising:
- adding a plurality of substrates;
- mixing a urea-formaldehyde (UF) resin or a melamine-urea-formaldehyde (MUF) resin, a lignosulfonate salt or a kraft lignin optionally with an amine and water at a pH of 5-11, preferably 6-10;
- optionally adding one or more additives to form the blended furnish,
- wherein the blended furnish has a buffer capacity of 2-200 mL of 0.1 N HCl by the Acid Titration Value (ATV) Method using 20 grams of blended furnish for a period of time up to 20 days.
1 more element
A method for preparing a blended furnish, comprising:
- adding a plurality of substrates;
- mixing a lignosulfonate salt or a kraft lignin with the substrates;
- adding a urea-formaldehyde (UF) resin or a melamine-urea-formaldehyde (MUF) resin optionally with an amine and water at a pH of 5-11, preferably 6-10;
- optionally adding one or more additives to form the blended furnish,
- wherein the blended furnish has a buffer capacity of 2-200 mL of 0.1 N HCl by the Acid Titration Value (ATV) Method using 20 grams of blended furnish for a period of time up to 20 days.
2 more elements
Dependencies are inferred from the claim text.