Color control and heat recuperation when producing activated clay
AssigneeFLSmidth A/S
InventorsRasmus Franklin Momme, Klaus Christian Thorslund
Life of this patent
Estimating the term…
Abstract
The invention relates to a method for producing a supplementary cementitious material for use in a cement product or concrete, the method comprising the steps of activating clay to the supplementary cementitious material at between 600 to 1000 degree Celsius; treating the activated supplementary cementitious material under reduced conditions to form a reduced product and cooling the reduced product to 300-400 degrees Celsius by a quenching process under oxidizing conditions.
Claims23
A method for producing a supplementary cementitious material for use in a cement product or concrete, the method comprising the steps of
- activating clay to the supplementary cementitious material at between 600 to 1000 degree Celsius;
- treating the activated supplementary cementitious material, after the activation of clay at a temperature between 600 to 1000 degrees Celsius, under reducing conditions to form a reduced product;
- and
- cooling the reduced product to a temperature in a range of 300 to 500 degrees Celsius, at a cooling rate with an average temperature change in the range of 10 to 100 degrees Celsius/second, by a quenching process under oxidizing conditions to rapidly slow and stop reaction kinetics of iron compounds that else can re-oxidize to Iron (III) species.
The method for producing a supplementary cementitious material according to claim-8, wherein said quenching process is performed with an air ratio of 0.01 to 20, such as 0.1 to 10, preferably 0.25 to 4.0 kg air/kg supplementary cementitious material to below 500 degrees Celsius and preferably 300 degrees Celsius.
Dependencies are inferred from the claim text.