Method for treating a wood substrate
AssigneeKoppers Performance Chemicals Inc.
InventorsJun Zhang, Peter Tham, Craig Wilson
Life of this patent
Estimating the term…
Abstract
A method for treating a wood substrate is provided. The method comprises contacting the wood substrate in a field application with an aqueous composition. The contacting is performed at a pressure of less than 20 psia. The aqueous composition comprises, by total weight of the aqueous composition, 1.0% to 10.0% by weight of a micronized basic copper carbonate, 0.35% to 2.5% by weight of a quaternary ammonium compound, and at least 80% by weight of water.
Claims21
A method for treating a pressure treated wood substrate, the method comprising:
- contacting the pressure treated wood substrate in a field application at a time of an initial installation of the pressure treated wood substrate with an aqueous composition by at least one of brushing and rolling, wherein the contacting is performed at a pressure of less than 20 psia, wherein the contacting is performed for a period of time suitable to inhibit fungal decay and insect attack of the pressure treated wood substrate, the aqueous composition comprising, by total weight of the aqueous composition:
- 1.0% to 10.0% by weight of a micronized basic copper carbonate;
- 0.35% to 2.5% by weight of a quaternary ammonium compound;
- and
- at least 80% by weight of water.
(canceled)
(canceled)
A method for treating a pressure treated wood substrate, the method comprising:
- physically altering at least a portion of the pressure treated dimensional lumber, thereby forming an exposed portion;
- contacting the exposed portion of the pressure treated dimensional lumber with an aqueous composition by at least one of brushing and rolling in a field application, wherein the contacting is performed at a pressure in a range of 12 psia to 16 psia, wherein the contacting is performed for a period of time suitable to inhibit fungal decay and insect attack of the pressure treated dimensional lumber, the aqueous composition consisting of, by total weight of the aqueous composition:
- 1.8% to 5.0% of a micronized basic copper carbonate that has an average particle size of 5 nanometers to 25 microns;
- 0.5% to 1.5% of a quaternary ammonium compound comprising dimethyldidecyl ammonium chloride, dimethyldidecyl ammonium carbonate, dimethyldidecyl ammonium bicarbonate, benzalkonium chloride, alkyl benzyl ammonium chloride, or a combination thereof;
- 85% to 95% of water, wherein the micronized basic copper carbonate is a solid suspended in the water;
- and
- optionally a colorant, an antifoam, a dispersant, a co-biocide, a water repellant, a wax, a mold inhibitor, a corrosion inhibitor, or a combination thereof.
Dependencies are inferred from the claim text.