Back to results
US 2023/0068164 A1Published application
3xx aluminum casting alloys, and methods for making the same
AssigneeAlcoa USA Corp.
InventorsXinyan Yan, Jen C. Lin
Life of this patent
Estimating the term…
Abstract
New 3xx aluminum casting alloys are disclosed. The aluminum casting alloys generally include from 6.5 to 11.0 wt. % Si, from 0.20 to 0.80 wt. % Mg, from 0.05 to 0.50 wt. % Cu, from 0.10 to 0.80 wt. % Mn, from 0.005 to 0.05 wt. % Sr, up to 0.25 wt. % Ti, up to 0.30 wt. % Fe, and up to 0.20 wt. % Zn, the balance being aluminum and impurities.
Claims3
A method, comprising:
- (a) shape casting a 3 xx aluminum casting alloy into a shape cast product, wherein the 3 xx aluminum casting alloy comprises:
- 6.5-11.0 wt. % Si;
- 0.20-0.80 wt. % Mg;
- 0.05-0.50 wt. % Cu;
- 0.10-0.80 wt. % Mn;
- 0.005-0.050 wt. % Sr;
- up to 0.25 wt. % Ti;
- up to 0.30 wt. % Fe;
- and
- up to 0.20 wt. % Zn;
- the balance being aluminum (Al) and impurities, wherein the 3 xx aluminum casting alloy includes not greater than 0.10 wt. % of any one impurity, and wherein the 3 xx aluminum casting alloy includes not greater than 0.35 wt. %, in total, of the impurities,
- wherein the shape casting step is selected from the group consisting of:
- high pressure die casting, gravity permanent mold casting, semi-permanent mold casting, squeeze casting, sand mold casting, centrifugal casting, and ablation casting;
- (b) optionally machining the shape cast product;
- (c) tempering the shape cast product, wherein, due to the tempering, the shape cast product is in a T temper.
12 more elements
Dependencies are inferred from the claim text.