0-99.9 wt % of a high heat copolycarbonate comprising high heat carbonate units derived from high heat bisphenol monomers comprising 1,1-bis(4-hydroxyphenyl)-3,3,5-trimethyl-cyclohexane, N-phenyl phenolphthalein bisphenol, 4,4′-(1-phenylethylidene)bisphenol, 4,4′-(3,3-dimethyl-2,2-dihydro-1H-indene-1,1-diyl)diphenol, 1,1-bis(4-hydroxyphenyl)cyclododecane, 3,8-dihydroxy-5a,10b-diphenyl-coumarano-2′,3′,2,3-coumarane, or a combination thereof, preferably 1,1-bis(4-hydroxyphenyl)-3,3,5-trimethyl-cyclohexane, N-phenyl phenolphthalein bisphenol, or a combination thereof, and optionally comprising low heat carbonate units, wherein a homopolycarbonate of the low heat carbonate units has a glass transition temperature of up to 150° C. as determined by differential scanning calorimetry as per ASTM D3418 with heating rate of 20° C./min;
- 0-55 wt % of a homopolycarbonate;
- 0.1-0.8 wt % of a C1-16 alkyl sulfonate salt flame retardant;
- optionally, 2-40 parts per million of an organosulfonic stabilizer of the formula
- wherein
- R7 is a C1-30 alkyl, C6-30 aryl, C7-30 alkylarylene, C7-30 arylalkylene, or a polymer unit
- derived from a C2-32 ethylenically unsaturated aromatic sulfonic acid or its ester,
- R8 is hydrogen, C1-30 alkyl;
- or a group of the formula —S(═O)2—R7;
- optionally, 0.1-5 wt % of an additive composition,
- wherein the amount of the high heat copolycarbonate, the C1-16 alkyl sulfonate salt flame retardant, the homopolycarbonate, the optional organosulfonic stabilizer and the optional additive composition is based on the total weight of the flame retardant composition, which sums to 100 wt %;
- wherein a molded sample of the flame retardant composition has
- a UL 94 rating of V0 at a thickness of 1.5 millimeter, and
- a transmission of greater than 80%, determined according to ASTM D1003 at a thickness of 1.0 millimeter, or
- a haze of less than 2%, determined according ASTM D1003 at a thickness of 1.0 millimeter.