Back to results
US 2023/0058012 A1Published application
All-solid-state battery with improved durability and method of manufacturing the same
AssigneesHyundai Motor Company, Kia Corporation
InventorsJae Min Lim, Hong Suk Choi, Sung Man Cho, Seon Hwa Kim, Young Jin Nam, Sang Wan Kim
Life of this patent
Estimating the term…
Abstract
Disclosed are an all-solid-state battery that may have uniform deposition of lithium and have excellent durability, and a method of manufacturing the same.
Claims14
An all-solid-state battery comprising:
- an anode current collector;
- a functional layer disposed on the anode current collector;
- a solid electrolyte layer disposed on the functional layer;
- and
- a cathode layer disposed on the solid electrolyte layer,
- wherein the functional layer comprises one or more components that forms an alloy or a compound with lithium, and comprises a first interfacial layer at a side of the solid electrolyte layer and a second interfacial layer at a side of the anode current collector,
- wherein a ratio (b/a) of a binding force (b) of the second interfacial layer to a binding force (a) of the first interfacial layer is about 0.6 or greater.
4 more elements
A method of manufacturing an all-solid-state battery, the method comprising:
- preparing a slurry comprising amorphous carbon, a metal powder, and a binder, wherein the metal powder forms an alloy with lithium;
- applying the slurry onto a substrate;
- primarily drying the substrate applied with the slurry at a first temperature for a first period;
- secondarily drying the primarily dried substrate applied with the slurry at a second temperature less than the first temperature for a second period greater than the first period to form a functional layer;
- and
- obtaining a structure in which the anode current collector, the functional layer, the solid electrolyte layer, and the cathode layer are sequentially laminated,
- wherein the functional layer comprises a first interfacial layer at a side of the solid electrolyte layer and a second interfacial layer at a side of the anode current collector,
- wherein a ratio (b/a) of a binding force (b) of the second interfacial layer to a binding force (a) of the first interfacial layer is about 0.6 or greater.
5 more elements