Ammoxidation catalyst for propylene, manufacturing method of the same catalyst, ammoxidation method using the same catalyst
AssigneeLG Chem, Ltd.
InventorsKyungyeon Kang, Ji Yeon Kim, Jun Seon Choi
Life of this patent
Estimating the term…
Abstract
The present disclosure relates to an ammoxidation catalyst for propylene, a manufacturing method of the same, and an ammoxidation method of propylene using the same. Specifically, in one embodiment of the present disclosure, there is provided a catalyst having a structure in which a metal oxide is supported on a silica support having a narrow particle size distribution, and excellent wear resistance.
Claims20
An ammoxidation catalyst for propylene comprising:
- a silica support containing a pore having a diameter of 2 to 15 nm and an apparent density of 0.25 to 1.0 g/cc;
- and
- a metal oxide supported on the silica support and comprising molybdenum (Mo), bismuth (Bi) and a dissimilar metal.
The ammoxidation catalyst of claim 46, wherein the catalyst comprises:
- a silica support containing a second pore;
- an inner coating layer continuously coating a wall surface of the second pore and comprising the metal oxide represented by the Chemical Formula 1;
- and
- a first pore positioned inside the second pore and occupying an empty space excluding the inner coating layer.
A manufacturing method of an ammoxidation catalyst for propylene comprising the steps of:
- preparing a first precursor aqueous solution containing a Mo precursor;
- preparing a second precursor aqueous solution containing a Bi precursor and a dissimilar metal precursor;
- supporting a mixture of the first and second precursor aqueous solutions on a silica support containing a pore having a diameter of 2 to 15 nm and an apparent density of 0.25 to 1.0 g/cc;
- drying the silica support on which the mixture of the first and second precursor aqueous solutions is supported;
- and
- calcining the dried material.
Dependencies are inferred from the claim text.