US 2023/0056012 A1Published application
Diamond Structures For Tooling
AssigneeAkhan Semiconductor, Inc.
InventorsAdam Khan, Kiran Kumar Kovi
Life of this patent
Estimating the term…
Abstract
A substrate for a tool including at least one sidewall includes at least one diamond layer. The diamond layer has a thickness between 10 nanometers and 1000 nanometers and is formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.
Claims37
A structure, comprising:
- a substrate having a surface including at least one sidewall;
- and
- a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.
A method for depositing a layer, comprising:
- providing a substrate having a surface including at least one sidewall;
- and
- depositing a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.
A wafer tooling structure, comprising:
- wafer tooling including a substrate having a surface including at least one sidewall;
- and
- a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.
A method for depositing a layer on wafer tooling, comprising:
- providing a wafer tool including a substrate having a surface that further includes at least one sidewall;
- and
- depositing a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.
Dependencies are inferred from the claim text.