Self-sintered thermal interface materials
AssigneeScience Applications International Corporation
InventorsJohn P. Timler, Xingcun C. Tong
Life of this patent
Estimating the term…
Abstract
Self-sintering thermal interface material is prepared from a polymer matrix and a filler. The polymer matrix may be a water or hydrogen peroxide or other water-contained solvent solution such as ammonia or alcohol containing a water soluble resin and fumed silica or an alcohol or other solvent solution containing at least one water insoluble resin and fumed silica. The filler contains i) gallium alkali metal or gallium metal, ii) one or more micro/nano-sized metallic fillers, and iii) dielectric fillers.
Claims30
A self-sintering thermal interface material comprising
- a polymer matrix and a filler;
- wherein the polymer matrix comprises a water or hydrogen peroxide solution comprising at least one water soluble resin and fumed silica;
- wherein the filler comprises i) gallium-alkali metal or gallium metal and ii) one or more micro/nano-sized metallic fillers.
A method of forming a self-sintering thermal interface material comprising:
- mixing a water-soluble resin and fumed silica with water, hydrogen peroxide, or water-contained ammonia or alcohol to form a water absorbing gel;
- and
- mixing the water absorbing gel with micro/nano-sized metallic fillers and gallium-alkali metal or gallium metal, at a temperature below the eutectic reaction temperature of the gallium-alkali metal or below the melting point of the gallium metal, to form a mixture.
A self-sintering thermal interface material comprising
- a polymer matrix and a filler;
- wherein the polymer matrix comprises an alcohol solution comprising at least one water insoluble resin and fumed silica;
- wherein the filler comprises i) gallium-alkali metal or gallium metal and ii) one or more micro/nano-sized metallic fillers.
A method of forming a self-sintering thermal interface material comprising:
- mixing a water-insoluble resin and fumed silica, dielectric filler, and micro/nano-sized metallic fillers with an alcohol solution or an equivalent solvent such as acetone, ionic liquids, NaOH/urea, ammonium hydroxide, phosphoric acid, acetic acid, formic acid, pyridine, aromatic hydrocarbons, halogenated hydrocarbons, and ketones;
- and
- mixing the alcohol solution with micro/nano-sized metallic fillers and gallium-alkali metal or gallium metal, at a temperature below the eutectic reaction temperature of the gallium-alkali metal or below the melting point of the gallium metal, to form a mixture.
Dependencies are inferred from the claim text.