Silicon carbide semiconductor device and method of manufacturing silicon carbide semiconductor device
AssigneeFuji Electric Co., Ltd.
InventorYasuyuki KAWADA
Life of this patent
Estimating the term…
Loading patent…
AssigneeFuji Electric Co., Ltd.
InventorYasuyuki KAWADA
Estimating the term…
After trench etching but before formation of a gate insulating film, a 15-minute to 60-minute heat treatment under a mixed gas atmosphere containing nitric oxide gas and nitrogen gas at a temperature from 1200 degrees C. to 1350 degrees C. and a 30-minute to 75-minute heat treatment under a nitrogen gas atmosphere held at the temperature of the 15-minute to 60-minute heat treatment are successively performed, oxidizing etching damage of inner walls of trenches. The total treatment time of the heat treatments includes a total time of at least 90 minutes when the temperature is a predetermined maximum temperature. The oxide layer of the trench inner walls is removed, exposing a clean face. Emission intensity of band edge emission for SiC obtained by CL analysis of surface areas of the inner walls of the trenches is at least equal to the emission intensity of the band edge emission for SiC obtained by the CL analysis of a surface free of dry etching.
A silicon carbide semiconductor device having an insulated gate with a three-layered structure including a gate, an oxide film, and a semiconductor, the silicon carbide semiconductor device, comprising:
A method of manufacturing a silicon carbide semiconductor device having an insulated gate with a three-layered structure including a gate, an oxide film, and a semiconductor, the method, comprising:
Dependencies are inferred from the claim text.