Method for forming a porous activited asphaltene material
AssigneeKing Fahd University of Petroleum and Minerals
InventorMOHAMMAD NAHID SIDDIQUI
Life of this patent
Estimating the term…
Abstract
A porous activated asphaltene material is described with a method of making and a method of using for the adsorption of a contaminant from a solution. The porous activated asphaltene material may be made by functionalizing solid asphaltene with nitric acid, and then treating the product with a metal hydroxide. The resulting porous activated asphaltene material exhibits a high porosity, and may be cleaned and reused for adsorbing contaminants.
Claims12
(canceled)
The method of claim 8, wherein the porous activated asphaltene material has an average particle size of 1-20 μm.
The method of claim 8, wherein the porous activated asphaltene material has a particle size distribution of 0.5-100 μm, wherein at least 60% of the particles have a particle size of 1-20 μm.
The method of claim 8, wherein the porous activated asphaltene material has a BET specific surface area of 2,000-4,700 m2/g.
The method of claim 8, wherein the porous activated asphaltene material has a BET specific surface area of 4,000-4,600 m2/g.
(canceled)
The method of claim 8, wherein the porous activated asphaltene material has a pore volume of 0.1-0.7 cm3/g.
A method for producing a porous activated asphaltene material, comprising:
- refluxing a solid asphaltene in nitric acid for 1-8 hours to produce a refluxed mixture;
- washing and drying the refluxed mixture to produce a functionalized asphaltene solid;
- grinding the functionalized asphaltene solid with a metal hydroxide to produce a ground mixture;
- heating the ground mixture at 300-1000° C. for 10-60 minutes to produce an activated powder;
- washing and drying the activated powder to produce the porous activated asphaltene material;
- wherein porous activated asphaltene material, comprises:
- an asphaltene compound having an elemental composition of 55-77 wt % C, 10-40 wt % O, 1-3 wt % S, 0.6-1.7 wt % H, and 0.2-1.2 wt % N each relative to a total weight of the asphaltene compound, wherein the asphaltene compound has at least one active group selected from the group consisting of an amine group, a nitro group, a carbonyl group, a carboxylic group and a hydroxyl group, the at least one active group covalently bonded to an asphaltene core,
- wherein the porous activated asphaltene material has a hierarchical porosity with a multi-modal pore distribution including first pores having a pore diameter in a range of 5-50 nm and second pores having a pore diameter of 3-5 μm, wherein the interior of the second pores connects with the first pores;
- and
- wherein the porous activated asphaltene material has a BET specific surface area of 1,000-4,800 m2/g.
12-30. (canceled)