Casting elements and methods of making the same using low temperature solidification
AssigneeRutgers, The State University of New Jersey
InventorsRichard E. Riman, Kevin Blinn
Life of this patent
Estimating the term…
Abstract
Foundry casting elements and methods of forming the same, the methods including: forming an aqueous slurry including an inorganic binder precursor, shaping the slurry using a pattern, curing the shaped slurry using a low temperature solidification process to form a casting element, and removing the pattern from the casting element.
Claims35
A method of forming a foundry casting element, the method comprising:
- forming an aqueous slurry comprising a solid inorganic binder material or a precursor thereof;
- shaping the slurry using a pattern;
- curing the shaped slurry at a temperature of less than 350° C. to form a casting element;
- and
- removing the pattern from the casting element,
- wherein the slurry optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder material or the precursor thereof.
A method of forming a foundry casting element, the method comprising:
- forming an aqueous first slurry comprising a refractory sand, colloidal silica and a binding polymer;
- forming an aqueous second slurry comprising a solid inorganic binder material and a thermoreversible additive;
- applying the first slurry to a pattern to form a first coating;
- heating the second slurry to a temperature ranging from about 40° C. to about 250° C.;
- dipping the pattern into the heated second slurry to form a second coating on the first coating;
- gelating the second coating by allowing the second coating to cool to a temperature below about 40° C.;
- and
- infiltrating the second coatings with CO2 to cure the coating to form a casting element with 2-coating layers;
- wherein the first slurry and/or second slurry optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder material or the binding polymer.
A foundry casting element, comprising:
- a refractory sand;
- and
- a binder comprising an aqueous magnesium aluminum phosphate gel admixed with one or more of clay, fumed silica and a soluble precursor of zinc or a rare earth lanthanide ion;
- and
- optionally an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder.
A refractory brick, castable, gunning or ramming mix, comprising MgO particles bonded to each other by magnesium carbonate particles, wherein the MgO particles are larger than the magnesium carbonate particles;
- and
- optionally an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the MgO particles and the magnesium carbonate particles.
A method of forming a foundry casting element, the method comprising:
- forming an aqueous slurry comprising a solid inorganic oxide material;
- and infiltrating the slurry with CO2 to at least partially convert the solid inorganic oxide material to a solid inorganic carbonate material and to form the foundry casting element or refractory element for bricks, castable, gunning, or ramming mixes;
- wherein the foundry casting element optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the inorganic oxide material.
Dependencies are inferred from the claim text.